HomeMatchup
Roofing glossary

Roofing Underlayment: What It Is, Types and Cost

The layer nobody sees and everybody argues about. Felt vs synthetic vs self-adhered, what the ASTM numbers mean, and when the code wants two layers instead of one.

Published by HomeMatchup editorial deskPublished July 29, 202610 min read

Roofing Underlayment at a glance

What it isA water-resistant sheet between the deck and the roof covering
Where it goesOver the roof deck, under shingles, tile, metal or shake
Typical materialAsphalt-saturated felt, synthetic polymer, or self-adhered membrane
Governing standardsASTM D226, D4869, D1970, D6757, D8257
Typical cost$0.05-$0.50/sq ft material; roughly $0.60-$2.70/sq ft installed
Code requirementRequired under roof coverings; two layers at 2:12-4:12 for shingles
Who installs itThe roofing crew, immediately after tear-off
Expected lifeFelt 12-20 yrs; synthetic 25-40 yrs
Commonly confused withIce and water shield, vapor barrier, house wrap

Quick answer: Roofing underlayment is a water-resistant sheet installed directly on the roof deck, beneath the shingles, tile, metal or shakes. It backs up the roof covering against wind-driven rain, protects the deck while the roof is open, and is required under roof coverings by the model building code. The three families are asphalt felt, synthetic, and self-adhered membrane.

What underlayment is and what it does

Underlayment is the layer between your roof deck and your roof covering. Nobody sees it once the shingles go on, and it’s the single most common place a cheap bid finds savings.

It does three jobs.

It’s the secondary water barrier. Shingles shed water, they don’t seal against it. In driving rain, water works sideways under the courses. Underlayment catches it and routes it back out over the drip edge. This is also what buys you time when a shingle blows off - the deck under it isn’t naked.

It protects the deck during installation. A tear-off leaves bare plywood or OSB exposed. Underlayment goes down the same day, often within the hour, so an afternoon thunderstorm doesn’t soak the decking you’re about to cover for the next 25 years.

It smooths the surface. Minor deck irregularities, small gaps and fastener heads telegraph less through a finished roof when there’s a uniform layer between them and the shingles.

What underlayment is not: it isn’t a vapor barrier, it isn’t a substitute for flashing, and it is not designed to serve as an exposed roof surface for months on end.

Where it sits in the roof assembly

From the framing up, a typical shingle roof stacks like this:

  1. Rafters or trusses - the structure
  2. Roof deck - plywood or OSB sheathing
  3. Ice barrier membrane at eaves, valleys and penetrations where required
  4. Underlayment across the remaining field
  5. Drip edge - under the underlayment at rakes, over it at eaves
  6. Starter strip along the eave
  7. Shingles, courses lapping upslope
  8. Ridge cap and ridge vent at the peak

Order matters. Underlayment is lapped shingle-fashion - each upper course over the one below, so water always runs onto the sheet beneath rather than into a seam. Get the sequence backwards anywhere and you’ve built a funnel.

The ice barrier goes down first at the eave, then the field underlayment laps over its upper edge. Where the two meet is one of the details worth looking at while your roof is open.

The three families of underlayment

Asphalt-saturated felt

The traditional product: a paper or fiberglass mat saturated with asphalt, sold as #15 and #30. It’s cheap, widely available and vapor-open, which some builders value for drying potential.

Here’s the fact almost no consumer page carries: the pound designations no longer describe the weight. Atlas Roofing reports #15 felt actually weighs 7.5 to 12.5 pounds per square and #30 weighs 16 to 27 pounds. The industry moved to type designations - ASTM D226 Type I for the lighter grade, Type II for the heavier - precisely because the old labels stopped meaning anything.

Felt’s weaknesses are real: it tears easily, wrinkles when it gets wet, becomes slick underfoot, and degrades quickly under sun. Atlas puts its perm rating at roughly 6 perms for #15 and 5 for #30 in dry-cup conditions, so it does breathe.

Synthetic underlayment

Woven or spun polypropylene or polyethylene. Bill Ragan Roofing describes the material difference plainly: felt is asphalt-soaked mat, synthetic is plastic fabric.

Synthetic weighs 40 to 100 grams per square meter, so a roll covers far more area for the same weight on a shoulder. It doesn’t tear, doesn’t wrinkle, has a walkable printed surface, and tolerates dramatically longer sun exposure.

The trade-off is vapor permeance: many synthetics are close to vapor-closed, which matters on assemblies that need to dry upward.

Self-adhered membrane

Peel-and-stick polymer-modified bitumen, governed by ASTM D1970. Its defining property, per ARMA, is that it seals around nail shanks - no other underlayment does. That’s why it’s the required product for ice barriers and the right choice for valleys, low-slope sections and around penetrations. Full detail in our ice and water shield guide.

What the ASTM numbers on the roll actually mean

Ask which standard your underlayment meets and you learn more than any brand name tells you. ARMA maps the whole set:

StandardCovers
ASTM D226Asphalt-saturated organic felt, Types I and II
ASTM D4869Steep-slope underlayment, includes a water-shedding requirement
ASTM D1970Self-adhering polymer-modified bituminous ice barrier
ASTM D6757Inorganic-fiber underlayment
ASTM D8257Mechanically attached polymeric (synthetic) underlayment

The current editions are ASTM D226/D226M-25 and ASTM D4869/D4869M-16a(2021).

The one to know is D4869 versus D226. D4869 adds a water-shedding performance requirement that D226 doesn’t have, which is why many building departments and manufacturers name it specifically. If a quote just says “felt,” ask which standard.

Felt vs synthetic: an honest comparison

Asphalt feltSynthetic
Material cost~$0.05-$0.10/sq ft~$0.17-$0.50/sq ft
Weight per square7.5-27 lbs40-100 g/m², much lighter
Tear resistanceLowHigh
Walkability when wetSlickTextured, better traction
Wrinkling when wetYesNo
UV exposure toleranceWeeks2-30 months by product
Vapor permeanceMore open (~5-6 perms dry-cup)Varies; many are near-closed
Expected service life12-20 years25-40 years

Service life figures are from Western States Metal Roofing. Note that the two credible sources we retrieved disagree on felt’s material price by roughly fivefold - Bill Ragan quotes about $0.25 per square foot where Western States quotes $0.05. Underlayment material pricing genuinely varies by market and grade, which is another reason the installed line item is a better basis for comparison than the roll price.

The practical verdict: for a shingle roof, synthetic is the default in 2026 and the upcharge is small relative to the total job. Felt remains defensible where vapor-openness is specifically wanted, or on budget-constrained repairs.

What the code requires, and where it varies

Underlayment is not optional. ARMA cites 2024 IBC §1507.1.1 and 2024 IRC §R905.1.1 as the sections mandating it under roof coverings.

The requirement that changes with your roof is the number of layers, and it’s driven by pitch:

  • Steeper than 4:12 - one layer
  • 2:12 to 4:12 - two layers cemented together, or a single self-adhering membrane in place of normal underlayment

The City of Hopkins, Minnesota publishes its adopted version of the asphalt shingle section: “For roof slopes from 2:12 to 4:12, double underlayment is required. Underlayment must conform to ASTM D 226 Type I, ASTM D 4869 Type I, or ASTM 6757.” Where two layers are used, they’re laid shingle-fashion with the upper overlapping the lower by roughly 19 inches - effectively a half-lap that gives two thicknesses everywhere.

Adoption varies by jurisdiction. States and municipalities adopt different code editions and amend them, and the acceptable underlayment type list is exactly where local amendments tend to appear. Confirm with your building department, and get the answer before material is ordered - the double-layer requirement is one of the easiest things for a low bid to leave out.

What it costs, and how it’s quoted

Underlayment is usually buried in a per-square roofing price rather than broken out. When it is broken out, published installed ranges run roughly $0.60 to $2.70 per square foot, or $60 to $270 per square, with self-adhered membrane at the top of the range.

The material is a small fraction of that. At $0.17-$0.25 per square foot for synthetic, the sheet on a 25-square roof is a few hundred dollars. The rest is labor: tear-off, hauling, cutting around penetrations, cap-nailing, and detailing at valleys and walls.

That cost structure has a practical consequence. Upgrading from felt to synthetic on a full reroof is one of the cheapest quality improvements available, because you’re only paying the material delta on labor you’re buying anyway. Ask what the line item costs before you decide it isn’t worth it - and run your area through the underlayment calculator to see how many rolls the job needs.

Doing it as a standalone job is the opposite: you’re paying full tear-off and reinstallation labor to change a $300 material. That’s why underlayment decisions are made at reroof time or not at all.

Common mistakes and misconceptions

“#15 felt weighs 15 pounds.” It weighs 7.5 to 12.5 pounds per square. The designation is nominal.

“Synthetic is waterproof.” It’s water-resistant and mechanically fastened. The cap nails holding it down are penetrations that do not self-seal. Only ASTM D1970 self-adhered membrane closes around a fastener.

Leaving it exposed past its rating. Every synthetic has a UV exposure window in its warranty - Owens Corning rates Titanium UDL50 at 180 days, while other products are rated at 60. Roofing over UV-degraded underlayment means the layer is already partly spent on day one. If your job stalls, find out what your product is rated for.

One layer on a 2:12 to 4:12 roof. This is the most consequential code miss on the list, and it’s invisible once the shingles are down.

Roofing over old underlayment. An overlay leaves the old layer buried. Whatever condition it’s in is the condition it stays in.

Treating underlayment as a leak fix. If water is getting in, the problem is almost always the covering, the flashing or the valley - not the underlayment. Underlayment is insurance, not a repair.

Assuming all synthetics are the same. UV rating, perm rating, tear strength and fastener requirements vary widely between products at very different prices.

How to check what’s on your roof

If your roof is currently being replaced, this is the one hour when you can actually see it. Go look after tear-off and before shingles.

  • Read the roll. The product name, the ASTM standard and the UV exposure rating are printed on it. Photograph it for your records.
  • Check the eaves. Is there a self-adhered membrane at the eave, and how far up does it go? See ice and water shield for what your climate requires.
  • Check the laps. Upper courses should overlap lower ones, never the reverse. Laps should be consistent, not eyeballed.
  • Check the valleys. Valleys should get membrane, centered and full length, not just field underlayment.
  • Check the fasteners. Cap nails or plastic-cap staples, not bare staples that pull through.

If the roof is already finished, you can sometimes see the underlayment edge from inside the attic at the eave, or at a gable overhang. Otherwise, your contract and the material invoice are your record - which is a good argument for having the underlayment product named in the contract rather than described as “felt or equivalent.”

The bottom line

Underlayment is a small line item that decides how your roof behaves in the two situations that matter most: the storm that drives water under the shingles, and the day a shingle goes missing. Synthetic outperforms felt on almost every practical measure for a modest material upcharge, and self-adhered membrane is the only product that seals around its own fasteners.

The decisions worth making deliberately are the product standard, the UV rating if the job might sit open, and - if your roof is between 2:12 and 4:12 - whether you’re actually getting the two layers the code calls for.

Planning a reroof? Get a free estimate and ask each contractor to name the underlayment product in writing.

Frequently asked questions

Roofing underlayment is a water-resistant sheet installed directly on the roof deck, underneath the shingles, tile, metal or shakes. It is the secondary water barrier: when wind-driven rain gets past the roof covering, or when the covering is briefly missing, the underlayment keeps water off the wood. It also protects the deck during installation.
Synthetic wins on most measures - it's lighter, far more tear-resistant, safer to walk on, doesn't wrinkle when wet, and tolerates much longer UV exposure. Felt costs less and is more vapor-open, which some builders prefer for drying potential. For most asphalt shingle roofs today, synthetic is the default and the modest upcharge is worth it.
No, not anymore. Atlas Roofing reports #15 felt weighs 7.5 to 12.5 pounds per roofing square and #30 felt weighs 16 to 27 pounds. The pound designations became nominal decades ago. The industry now specifies by type - ASTM D226 Type I for the lighter grade and Type II for the heavier - rather than by the old weight labels.
On asphalt shingle roofs steeper than 4:12, one layer. Between 2:12 and 4:12, the model code requires two layers cemented together, or a single self-adhered membrane in their place. Adoption varies by jurisdiction and some building departments amend the rule, so confirm locally before ordering material.
Material alone is cheap. Western States Metal Roofing puts #15 felt around $0.05 per square foot, #30 felt around $0.10, and synthetic at $0.17-$0.25. Installed as its own line item, published ranges run roughly $0.60-$2.70 per square foot, because most of the cost is labor and tear-off, not the sheet itself.
It depends entirely on the product, and it's a warranty term rather than a material property. Western States Metal Roofing puts synthetics at anywhere from 2 to 30 months. Owens Corning rates Titanium UDL50 at 180 days of UV exposure. Felt degrades far faster - assume weeks, not months, in direct sun.
Yes. Metal panels expand, contract and can condense moisture on their underside, so the underlayment is doing real work. High-temperature synthetic or self-adhered products are typically specified because metal roofs run hotter than shingles. Follow the panel manufacturer's installation instructions, which will name acceptable underlayment types.
ARMA maps them: ASTM D226 covers asphalt-saturated organic felt, D4869 covers steep-slope underlayment with a water-shedding requirement, D1970 covers self-adhering polymer-modified bituminous ice barrier, D6757 covers inorganic-fiber underlayment, and D8257 covers mechanically attached synthetic underlayment. Ask which standard the product on your quote meets.
Water-resistant, not waterproof. Synthetic is mechanically fastened with cap nails or staples, and those penetrations do not self-seal. Only a self-adhered ASTM D1970 membrane seals around nail shanks. That difference is exactly why ice barrier membrane goes on the vulnerable areas and synthetic covers the field.
On a full tear-off, yes - the old underlayment comes off with the shingles and new goes down on the bare deck. If a contractor proposes shingling over existing layers, the old underlayment stays buried and you get none of the benefit of new material. A tear-off is also the only way anyone sees the deck condition.
It can be, and some contractors do it, but it is not automatically better. A full-coverage self-adhered membrane has very low vapor permeance, so on a deck that cannot dry to the inside it can trap moisture. It's a reasonable choice on low-slope sections and a debated one across an entire vented attic roof.
Underlayment sits on top of the roof deck and keeps liquid water out. A vapor retarder sits on the warm side of the insulation, usually at the ceiling plane, and slows water vapor from moving into the assembly. They solve opposite halves of the same moisture problem and are not substitutes for one another.
It buys you time, not immunity. Underlayment sheds water that gets past the shingles and protects the deck during a storm or while the roof is open. It is not designed to be a permanent exposed roof surface, and it will not compensate for missing flashing, bad valley detailing, or a roof covering at the end of its life.
Three things. It backs up the shingles against wind-driven rain that works under the courses. It protects the deck during the hours or days the roof is open during installation. And it provides a smooth, uniform surface so minor deck irregularities don't telegraph through the finished roof.
Manufacturers specify acceptable underlayment in their installation instructions, and using a non-approved product can affect coverage - particularly on enhanced or system warranties that require the manufacturer's own components. Ask your contractor which system warranty they're registering and what it requires before the material is ordered.

Sources

  1. Steep Slope Roofing Underlayment (types, ASTM standards, code sections)Asphalt Roofing Manufacturers Association (ARMA)
  2. Weights and Measures of Underlayment for RoofingAtlas Roofing
  3. Synthetic vs. Felt Roof Underlayment: Which Should I Use?Western States Metal Roofing
  4. Felt Underlayment vs. Synthetic UnderlaymentBill Ragan Roofing
  5. ASTM D4869/D4869M-16a(2021) - Asphalt-Saturated Organic Felt UnderlaymentASTM International
  6. ASTM D226/D226M-25 - Asphalt-Saturated Organic Felt Used in RoofingASTM International
  7. Asphalt Shingles R905.2 (adopted code page, double underlayment rule)City of Hopkins, Minnesota
  8. Titanium UDL50 synthetic underlayment (UV exposure rating)Owens Corning

Costs and lifespans are 2026 US ranges and vary by region, product line, slope, and installer. Confirm with a local pro before deciding.

Who wrote and checked this

Published by

HomeMatchup editorial desk

Editorial

The technical claims on this page were checked against installation practice before publication. Written and edited by the HomeMatchup editorial desk. No named reviewer yet. Sources dated. Report a correction.

Get matched before you rush.

Free quotes from businesses that serve your area.

Free · No obligation

(866) 582-8523 Get free quotes